SLS: laser sintering of plastic powder
Selective laser sintering explained: process, materials such as PA12, achievable tolerances, design rules, surfaces and typical uses.
As of November 2026
In selective laser sintering (SLS) a laser fuses fine plastic powder layer by layer. Unfused powder stays in place and supports the part. SLS therefore needs no support structures and allows shapes that other processes can hardly make.
The process
- A roller or blade spreads a thin layer of powder, about 0.1 mm.
- The build chamber is preheated to just below the melting point.
- A laser traces the cross-section of the part and fuses the powder.
- The platform drops and the next layer follows.
- After printing, the whole powder block has to cool slowly, often for as long as the print took.
- The parts are dug out and cleaned with compressed air or blasting media.
Part of the unused powder is mixed with fresh powder and reused.
Materials
| Material | Property | Typical use |
|---|---|---|
| PA12 | balanced, dimensionally stable, chemical-resistant | the standard for functional parts |
| PA11 | tougher, higher elongation, bio-based | snap hooks, hinges, orthoses |
| PA12 glass-filled | stiffer, more heat-resistant | housings, jigs |
| TPU | elastic | seals, dampers, soles |
| PP | chemical-resistant, light | containers, ducts |
Typical values
| Quantity | Usual range |
|---|---|
| Layer height | 0.08 to 0.12 mm |
| Dimensional tolerance | about ±0.3 mm or ±0.3 % |
| Minimum wall thickness | 0.7 to 1.0 mm |
| Smallest detail | about 0.5 mm |
| Clearance for moving parts | from 0.5 mm |
Design rules
- Powder has to get out. Cavities need openings of at least 4 mm, preferably two.
- Even wall thickness. Thick masses warp and sink.
- Avoid large flat areas or stiffen them with ribs. They tend to warp.
- Moving assemblies in one piece are possible: chains, hinges and joints print ready-assembled.
- Lettering from 1 mm stroke width, raised or engraved by at least 0.5 mm.
Surface and finishing
SLS parts are matt and slightly rough, like fine sandpaper. The base colour is white or grey. Common steps:
- Blasting for cleaning and smoothing
- Dyeing in a bath, usually black
- Vibratory finishing for smoother faces
- Chemical smoothing, which seals the surface and makes it wipeable
- Painting for visible parts
Strengths
- no supports, great design freedom
- almost equal strength in all directions
- robust, long-lasting parts fit for end use
- many parts in one build, hence economical in series
Limits
- rough, porous surface without treatment
- longer lead time because of cooling
- machines are expensive, so the process is almost only available from service providers
- fewer colours than FDM
What SLS is the first choice for
Functional parts in small series, housings with snap hooks, air ducts, brackets in vehicles, orthopaedic aids, complex assemblies in one piece.
FAQ
Are SLS parts watertight?
From about 1.5 mm wall thickness they resist splashing water. For permanently tight containers, sealing or chemical smoothing is advisable.
Why does a single SLS part cost more than an FDM part?
The build chamber has to be filled, heated and cooled. The unit price only drops clearly when many parts are printed together.
More topics
- FDM / FFFPlastic filament is melted and laid down in lines. The most widespread process.
- SLA / resinLiquid resin is cured with light. For the finest detail and smooth faces.
- MJFPowder is fused across the whole layer with ink and heat. Fast and series-ready.
- MetalLaser melting and related processes for steel, aluminium and titanium.