Post-processing: sanding, smoothing, painting and joining 3D prints
All the common finishing steps for FDM, resin and powder parts: removing supports, sanding, filling, painting, chemical smoothing, gluing and setting threaded inserts.
As of November 2026
Few prints are finished straight off the machine. How much finishing makes sense depends on the purpose: a bracket in the workshop needs none, a presentation model a lot.
The steps in a sensible order
- Remove supports. With side cutters, pliers or a scalpel. On resin parts do this before post-curing; they come off more easily.
- Deburr. Clean edges and the first layer with a deburring tool or knife.
- Sand. From coarse to fine: 120 or 180 grit, then 240, 400 and 600. Wet sanding stops the plastic warming up and smearing.
- Fill and prime. Spray filler closes the grooves between layers. Two or three thin coats, sanding finely in between.
- Paint. Primer, colour coat, clear coat. Acrylic paints are uncomplicated; spray cans or an airbrush give the smoothest finish.
- Polish or seal. Clear coat or epoxy protects and adds gloss.
Chemical smoothing
- ABS and ASA can be smoothed with acetone vapour. The surface melts slightly and turns glossy. Details round off in the process. Acetone is highly flammable, so this belongs outdoors or under extraction.
- PLA and PETG do not react to acetone. Only sanding and filling or a coating help here.
- Powder-bed nylon parts are smoothed industrially with solvent vapour. That seals the pores and makes them wipeable.
Joining
| Method | Suitable for | Note |
|---|---|---|
| Superglue | PLA, PETG, resin | fast, brittle seam |
| Two-part epoxy | almost everything | strong, fills gaps |
| Solvent cement, acetone | ABS, ASA | welds the parts |
| Plastic welding | PLA, PETG | with a soldering iron or 3D pen |
| Screws and inserts | loaded joints | detachable |
Threaded inserts
Knurled brass inserts are melted into a pre-printed hole with a soldering iron. They hold far more than a printed thread and survive frequent screwing. The hole is designed slightly smaller than the insert's outer diameter; the maker states the dimensions.
Annealing
Some plastics are heat-treated in an oven after printing. That raises heat resistance and relieves stress. The part shrinks and warps slightly, so annealing only suits non-critical dimensions.
What you can realistically expect
An injection-moulded look is possible with FDM but costs hours of manual work. For visible parts in quantity, another process is often more economical than elaborate finishing.
FAQ
Which paint sticks to 3D prints?
Acrylic paints and spray paints stick well after sanding and priming. Adhesion on TPU and nylon is harder; special primers help.
Can 3D prints be made dishwasher-safe?
Not PLA; it deforms. PETG and ASA cope better with the temperature, but the grooves remain hard to clean.
Our own service: The finishing 3D Druck Berlin offers is described under tolerances, surfaces and finishing. For sealed brand objects see Brandform: material, colour, finish.
More topics
- Design rulesGuide values for walls, overhangs, holes, lettering and joints.
- Tolerances and fitsWhat accuracy is realistic and how to design fits.
- Slicer settingsWhich setting does what, and where to start.
- Fixing print defectsThe typical faults, their causes and what helps.
- CAD programsFrom browser building blocks to parametric CAD: what suits whom.
- 3D scanningPhotogrammetry, structured light, laser: what a scan delivers and where it ends.
- The first printFrom unboxing to the first successful part.
- Buying a 3D printerDesigns, features, price classes and running costs, without brand advertising.
- Finding modelsWhere ready-made 3D models are and how to spot good ones.