Understanding slicer settings: layer height, walls, infill, supports
The main slicer settings explained, with their effect on quality, strength and print time, and sensible starting values.
As of November 2026
The slicer is the program that turns a 3D model into print paths. Its settings shape the result more than the printer itself. If you order from a service, you will meet the same terms in the quote.
The six most important settings
Layer height
It determines how fine the steps on slopes are, and affects print time almost linearly.
| Layer height | Effect | Typical for |
|---|---|---|
| 0.08 to 0.12 mm | very fine, long print time | figures, visible parts |
| 0.16 to 0.2 mm | a good compromise | most parts |
| 0.24 to 0.3 mm | fast, visibly stepped | large parts, functional samples |
Wall lines
The number of outer lines. Two are enough for models, three to four for loaded parts. Walls contribute most to strength.
Infill
Given as a percentage. 10 to 15 percent is enough for display models, 20 to 40 percent for functional parts. Above 50 percent adds little strength relative to time and material.
Common patterns: grid (fast), gyroid (even in every direction), honeycomb (strong, slower), cubic (a good all-rounder).
Top and bottom layers
The number of closed layers above and below. As a rule of thumb, top and bottom should each be about 0.8 to 1 mm thick so the infill pattern does not show through.
Supports
- Normal supports: a lattice under the overhang, stable, leave more marks
- Tree supports: branching limbs, save material and come off more easily
- Threshold angle: the slope from which supports are added, usually 45 to 50 degrees
Bed adhesion
- Skirt: a line around the part, only to prime the nozzle
- Brim: a flat rim on the part that prevents warping
- Raft: a complete base, rarely needed today
Other settings worth knowing
- Seam: sets where each layer starts. Hidden in an edge, it is hardly noticeable.
- Cooling: lots of fan for PLA, little for PETG, almost none for ABS and ASA.
- Speed: print outer walls slower than infill for a better surface.
- Ironing: the nozzle passes over the top face again and levels it.
- Variable layer height: fine on curves, coarse on vertical walls.
Orientation first
Before changing numbers, the position of the part should be right. Three questions help:
- Which face lies flat on the plate?
- Where does the force act, and do the layers run along it?
- Which face is visible and should stay free of supports?
Sensible starting values
| Setting | Value |
|---|---|
| Layer height | 0.2 mm |
| Wall lines | 3 |
| Infill | 15 to 20 %, gyroid or grid |
| Top and bottom | 4 to 5 layers |
| Supports | only where needed, tree supports |
| Adhesion | skirt, brim if warping occurs |
FAQ
Does more infill always make a part stronger?
Noticeably up to about 40 percent, hardly beyond. One extra wall line usually does more than ten percentage points of infill.
Which slicer is the right one?
The common free programs all give good results. For beginners the printer maker's own slicer is easiest, because its profiles are tuned.
Our own service: If you have a finished file and would prefer to skip the settings, upload it to 3D Druck Berlin: print my STL.
More topics
- Design rulesGuide values for walls, overhangs, holes, lettering and joints.
- Tolerances and fitsWhat accuracy is realistic and how to design fits.
- Post-processingFrom raw print to finished part: sanding, painting, gluing, inserts.
- Fixing print defectsThe typical faults, their causes and what helps.
- CAD programsFrom browser building blocks to parametric CAD: what suits whom.
- 3D scanningPhotogrammetry, structured light, laser: what a scan delivers and where it ends.
- The first printFrom unboxing to the first successful part.
- Buying a 3D printerDesigns, features, price classes and running costs, without brand advertising.
- Finding modelsWhere ready-made 3D models are and how to spot good ones.